Contact us
- : 0086-21-61182423
- : 0086-21-61182425
- : [email protected]
- : Room 301,Unit 6,lane 2500,xiupu Road,Kangqiao Industrial Area,Pudong New District,Shanghai
HOT News
- Improper welding of X80 pipeline may cause cracks
- Brief introduction of API X52 pipeline steel
- The difference between PSL1 and PSL2
- Harm of inclusions in X70 pipeline steel
- API 5L pipeline pipe
- X52 steel plate surface quality standards that need to be met
- The basic production process of API 5L X60 pipeline steel
- The key to Q460D steel welding process
- What does the heat treatment of Q690 Steel include?
- Reasons for choosing Q690D steel
CCS DH32 steel plate for shipbuilding and ocean engineering
Posted:2019-10-09 14:31:47
CCS DH32 steel plate is mainly used to build vessels which are sailing in low temperature oceans. CCS DH32 steel plate owns the minimum yield strength of 45,500 psi (315 MPa), and ultimate tensile strength of 64,000 - 85,000 psi (440-590 MPa).
CCS DH32 steel plate chemical composition:
Grade | C % | Si % | Mn % | P % | S % | V % | AL % | Cr % |
CCS DH32 | 0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.05-0.10 | 0.015 | 0.20 |
Cu % | Mo % | Nb % | Ni % | Ti % | ||||
0.35 | 0.08 | 0.02-0.05 | 0.40 | 0.02 |
CCS DH32 steel plate mechanical properties:
Grade | Rm (MPa) | Re(MPa) min | A% min | Akv/J min | ||||||
E.T °C | Thickness (mm) | |||||||||
≤ 50 | > 50-70 | > 70-100 | ||||||||
L | C | L | C | L | C | |||||
CCS DH32 | 440-570 | 315 | 22 | -20 | 31 | 22 | 38 | 26 | 46 | 31 |
CCS DH32 steel plate delivery condition has relation to the thickness. Normally for CCS DH32 steel plate thickness belows 40 millimeters, the delivery condition under As rolled is Ok. And for CCS DH32 steel plate thickness equal and above 40mm, it shall be under TMCP or Normalized delivery condition.