- : 0086-21-61182423
- : 0086-21-61182425
- : [email protected]
- : Room 301,Unit 6,lane 2500,xiupu Road,Kangqiao Industrial Area,Pudong New District,Shanghai
- Improper welding of X80 pipeline may cause cracks
- Brief introduction of API X52 pipeline steel
- The difference between PSL1 and PSL2
- Harm of inclusions in X70 pipeline steel
- API 5L pipeline pipe
- X52 steel plate surface quality standards that need to be met
- The basic production process of API 5L X60 pipeline steel
- The key to Q460D steel welding process
- What does the heat treatment of Q690 Steel include?
- Reasons for choosing Q690D steel
What is JIS G3101 SS400 equivalent ASTM steel
JIS G3101 SS400 steel is widely used low carbon steel. There are various steel grades equivalent to SS400 steel in foreign standards. JIS G3101 SS400 equivalent ASTM steel materials are A36 steel, A283 Gr C steel ( A283C / A283 grade C). Below is about JIS G3101 SS400 equivalent ASTM steel chemical composition and mechanical properties.
JIS G3101 SS400 equivalent ASTM steel chemical composition:
Grade | C (t≤16mm) | Si | Mn | P | S | Cu |
SS400 | - | - | - | 0.050 max | 0.050 max | - |
A36 | 0.26 max | 0.40 max | - | 0.040 max | 0.050 max | 0.20 min |
A283 Gr C | 0.24 max | 0.04 max | 0.09 max | 0.035 max | 0.040 max | 0.20 min |
JIS G3101 SS400 equivalent ASTM steel mechanical properties:
Grade | Yield strength ReH/(N/mm2) | Tensile strength Rm/(N/mm2) | Elongation A/% |
(t≤16mm) min | (3mm≤t≤16mm) | (3mm≤t≤40mm) min | |
SS400 | 245 | 400-500 | 21 |
A36 | 250 | 400-550 | 23 |
A283 Gr C | 205 | 380-515 | 25 |
JIS G3101 SS400 equivalent ASTM steel chemical composition and mechanical properties are close to those of SS400 steel. That is the most reason why they are regarded as equivalent grades. We supply SS400 steel, A36 steel, A283 Gr C steel and so on steel materials all over the world. Welcome to consult steel price and any information about steel materials.