- : 0086-21-61182423
- : 0086-21-61182425
- : [email protected]
- : Room 301,Unit 6,lane 2500,xiupu Road,Kangqiao Industrial Area,Pudong New District,Shanghai
- Improper welding of X80 pipeline may cause cracks
- Brief introduction of API X52 pipeline steel
- The difference between PSL1 and PSL2
- Harm of inclusions in X70 pipeline steel
- API 5L pipeline pipe
- X52 steel plate surface quality standards that need to be met
- The basic production process of API 5L X60 pipeline steel
- The key to Q460D steel welding process
- What does the heat treatment of Q690 Steel include?
- Reasons for choosing Q690D steel
China 302 Stainless Steel,302 Stainless Steel price
shanghai katalor can supply Alloy 302 (UNS S30200) in sheet, sheet coil, plate, round bar, processed flat bar and tubular products.
General Properties
Alloy 302 is a variations of the 18% chromium / 8% nickel austenitic alloy, which is the most familiar and the most frequently used in the stainless steel family. Alloy 302 is a slightly higher carbon version of 304, often found in strip and wire forms. It is a tough, ductile grade that demonstrates comparable corrosion resistance, is non-magnetic, and is not hardenable by heat treatment. Alloy 302 is usually used in its annealed condition and has a high ease of fabrication and formability.
Specifications: UNS S30200
Applications:
Although many applications have shifted to 304 and 304L due to advances in melting technology, availability, and cost, Alloy 302 is still used in a variety of industries. Some examples include:
- Stamping
- Spinning
- Wire forming
- Formed into all types of washers, springs, screens, and cables
- Food and beverage industry
- Pressure containing applications
- Sanitary or cryogenic applications
Some examples of products that are partially or completely constructed of 302 include:
- Blenders
- Counters
- Dish racks
- Dishwashers
- Refrigerators
- Washing machines
Standards:
- ASTM/ASME: UNS S30200
- EURONORM: FeMi35Cr20Cu4Mo2
- DIN: 2.4660
Chemical Properties:
C | Mn | Si | P | S | Cr | Ni | N | |
---|---|---|---|---|---|---|---|---|
302 | max: 0.15 | max:2.0 | max: 0.75 | max: 0.045 | max: 0.03 | min: 17.0 max: 19.0 | min: 8.0 max: 10.0 | max: 0.10 |
Mechanical Properties:
Grade | Tensile Strength ksi (min) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Rockwell B) MAX |
---|---|---|---|---|
302 | 75 | 30 | 40 | 92 |
Physical Properties:
Density lbm/in3 |
Thermal Conductivity (BTU/h ft. °F) |
Electrical Resistivity (in x 10-6) |
Modulus of Elasticity (psi x 106 |
Coefficient of Thermal Expansion (in/in)/ °F x 10-6 |
Specific Heat (BTU/lb/ °F) |
Melting Range (°F) |
---|---|---|---|---|---|---|
at 68°F: 0.285 | 9.4 at 212°F | 72.0 at 70°F | 28 | 9.6 at 32 – 212°F | 0.1200 at 32°F to 212°F | 2500 to 2590 |
12.4 at 932 °F | 10.2 at 32 – 1000°F | |||||
10.4 at 32 – 1500°F |