- : 0086-21-61182423
- : 0086-21-61182425
- : [email protected]
- : Room 301,Unit 6,lane 2500,xiupu Road,Kangqiao Industrial Area,Pudong New District,Shanghai
- Improper welding of X80 pipeline may cause cracks
- Brief introduction of API X52 pipeline steel
- The difference between PSL1 and PSL2
- Harm of inclusions in X70 pipeline steel
- API 5L pipeline pipe
- X52 steel plate surface quality standards that need to be met
- The basic production process of API 5L X60 pipeline steel
- The key to Q460D steel welding process
- What does the heat treatment of Q690 Steel include?
- Reasons for choosing Q690D steel
E36-3 steel plate,E36-3 price,NFA AE 255 B,C,D steel properties
E36-3 steel plate
Steel Category: structural steel
Steel standard:NFA 35-501
Steel grade:NFA 35-501 E36-3
Dimension: Thickness 5-300mm, Width 1500-3500mm, Length 3000-12000mm
Application: Mainly used in many applications, combining good welding properties with guaranteed strengths and the uses varied including civil and industrial engineering.
E36-3 steel chemical composition
Grade |
C≤16mm max |
C>16mm max |
Si max |
Mn max |
P max |
S max |
N max |
E36-3 |
0.20 |
0.20 |
0.55 |
1.60 |
0.040 |
0.040 |
- |
E36-3steel mechanical property
Grade |
Yield Strengh ReH[N/m㎡] Transv. min |
Tensile Strength ReH[N/m㎡] Transv. |
Fracture Elongation [%] Transv.min A80 A5 |
Notch Impact Energy3) Ch V. Complete sample Longitud.min[J] |
|||||||
|
≤16 mm |
>16 mm |
<3 mm |
≥3 mm |
Up to 1.50 mm |
1.50- 2.00 mm |
2.01- 2.50 mm |
2.51- 2.99 mm |
≥3 mm |
Temp. [℃] |
AV [J] |
E36-3 |
355 |
345 |
510- 680 |
490- 630 |
13 |
14 |
15 |
16 |
20 |
0 |
27 |
Katalor STEEL sells E36-3 in NFA 35-501 standard. If you have any need in this steel grade, please inquiry us soon.