Contact us
- : 0086-21-61182423
- : 0086-21-61182425
- : [email protected]
- : Room 301,Unit 6,lane 2500,xiupu Road,Kangqiao Industrial Area,Pudong New District,Shanghai
HOT News
- Improper welding of X80 pipeline may cause cracks
- Brief introduction of API X52 pipeline steel
- The difference between PSL1 and PSL2
- Harm of inclusions in X70 pipeline steel
- API 5L pipeline pipe
- X52 steel plate surface quality standards that need to be met
- The basic production process of API 5L X60 pipeline steel
- The key to Q460D steel welding process
- What does the heat treatment of Q690 Steel include?
- Reasons for choosing Q690D steel
EN 10113-3 S275M steel specification,EN 10113-3 S275M material equivalent
EN 10113-3 S275M steel specification:
EN 10113-3 S275M requirements for flat products with nominal thickness ≤63mm and long products with nominal thickness ≤150mm of hot-rolled weldable fine grain structural steels.
EN 10113-3 standard is hot-rolled products in weldable fine grain structural steels,part 3,delivery conditions for thermomechanical rolled steels.
S275M material chemical composition:
Grade | C max |
Si max |
Mn max |
P max |
S max |
N max |
AL max |
Nb max |
V max |
Ti max |
Cr max |
Ni max |
Mo max |
Cu max |
CEV max |
S275M | 0.13 | 0.50 | 1.5 | 0.035 | 0.03 | 0.015 | 0.02 | 0.05 | 0.08 | 0.05 | 0.30 | 0.3 | 0.20 | 0.55 | 0.38 |
EN 10113-3 S275M steel impact energy:
Min value of impact energy for impact tests on longitudinal V-notch test pieces for M steels
Grade | Min values of impact energy in J at test temperatures,in OC | ||||||
+20 | 0 | -10 | -20 | -30 | -40 | -50 | |
S275M | 55 | 47 | 43 | 40 | -- | -- | -- |
EN 10113-3 S275M steel in stock,and we also can supply EN 10113-3 S275M steel equivalent material,if you need EN 10113-3 S275M steel supplier,EN 10113-3 S275M steel,please feel free to contact katalor!