- : 0086-21-61182423
- : 0086-21-61182425
- : [email protected]
- : Room 301,Unit 6,lane 2500,xiupu Road,Kangqiao Industrial Area,Pudong New District,Shanghai
- Improper welding of X80 pipeline may cause cracks
- Brief introduction of API X52 pipeline steel
- The difference between PSL1 and PSL2
- Harm of inclusions in X70 pipeline steel
- API 5L pipeline pipe
- X52 steel plate surface quality standards that need to be met
- The basic production process of API 5L X60 pipeline steel
- The key to Q460D steel welding process
- What does the heat treatment of Q690 Steel include?
- Reasons for choosing Q690D steel
EN 10113-3 S275ML
S275ML steel plate/sheet, EN 10113-3 S275ML steel plate/sheet, S275ML steel plate/sheet supplier/Chinese supplier, S275ML steel plate/sheet price, S275ML steel plate/sheet mechanical property.
EN 10113-3 S275M steel equivalent grades:
S275ML steel plate/sheet is in EN 10113-3 standard, the grade number is 1.8819. The equivalent materials of S275ML steel are DIN-SEW083 TStE 275 TM, UNI 7382 Fe E 275 KTTM.
S275ML |
Comparision of steel grades |
|
DIN-SEW083 |
TStE 275 TM |
|
UNI 7382 |
Fe E 275 KTTM |
|
BS 4360 |
- |
|
ASTM |
- |
EN 10113-3 S275ML steel chemical composition %:
Main chemical composition in EN 10113-3 S275ML steel is carton max 0.13, silicon max 0.50, manganese max 1.50, phosphorus max 0.025, Sulphur max 0.02, chromium max 0.30. More detailed information about S275ML steel, please refer to the down table:
Grade |
C |
Si |
Mn |
P |
S |
N |
AL |
Nb |
V |
Ti |
Cr |
Ni |
Mo |
Cu |
CEV |
S275ML |
0.13 |
0.50 |
1.5 |
0.025 |
0.02 |
0.015 |
0.02 |
0.05 |
0.08 |
0.05 |
0.30 |
0.3 |
0.10 |
0.55 |
0.38 |
EN 10113-3 S275ML steel mechanical property:
EN10113 S275ML is a technical delivery conditions for thermomechanical rolled weldable fine grain structural steels.It is according to EN10113-3 standard.S means the structural steel, M means the delivery condition. Capital letter L for the quality with specified minimum values of values of impact energy at temperature not lower than -50 degree.
Temperature |
-50 |
-40 |
-30 |
-20 |
-10 |
0 |
20 |
Notch impact test. Min. absorbed energy |
27 |
31 |
40 |
47 |
51 |
55 |
63 |
Nominal thickness(mm) |
to 16 |
16-40 |
40-63 |
63-80 |
80-100 |
100-120 |
ReH-Minimun yield strength(Mpa) |
275 |
265 |
255 |
245 |
245 |
240 |
Nominal thickness(mm) |
to 40 |
40-63 |
63-80 |
80-100 |
100-120 |
Rm-Tensile strength(Mpa) |
370-530 |
360-520 |
350-510 |
350-510 |
350-510 |
Nominal thickness(mm) |
- |
||||
A-Minimum elongation |
24 |
Shanghai Katalor Industry Co., Ltd Will return you with high-quality products and complete after-sale service with the lowest price. we committed to exceed customer’s expectation on the basis of quality, price, and delivery. We sincerely hope to establish long-term cooperation relationship with you on the basis of mutual benefit, reciprocity and common development.As S275ML Mechanical and S275ML suppliers,we can supply S275ML Chemical,S275ML Mechanical and S275ML standard for you ,please click to contact us