- Performance that API 5L X52 PSL2 pipeline steel should have
- Surface Quality Requirements of EH40 Steel plate
- Excellent properties and applications of EH40 shipbuilding Steel
- Influence of gas in 50CrMo4 steel plate
- Cause of Quenching Cracks in 50CrMo4
- Factors Affecting Welding Toughness of
- Z direction performance of EH32 steel plate
- Features of AR450 wear-resistant plate
- Characteristics of NM500 wear-resistant plate
- Harm of inclusions in API 5L X42 pipeline steel
EN10155 S235J2W S235J2WP
S235J2W S235J2WP,S235J2W,S235J2WP steel plate,EN S235J2W S235J2WP steel,EN10155 S235J2W,S235J2WP steel plate/sheet, EN10155 S235J2W,S235J2WP steel plate/sheet for atmospheric corrosion resistance, S235J2W,S235J2WP carbon steel used for resisting atmospheric corrosion , EN10155 steel plate for atmospheric corrosion resistance,S235J2W,S235J2WP steel supplier
/Chinese supplier, S235J2W,S235J2WP steel price...
Equivalent grade :
S235J2W,S235J2WP steel plate/sheet is in EN10155 standard. It's grade Number is 1.8961. The equal material of S235J2W,S235J2WP is: SEW087 WTST 37-3 , NFA 35-502 E24W4, UNI Fe360DK.
S235J2WP |
SEW087 |
WTST 37-3 |
NFA 35-502 |
E24W4 |
|
UNI |
Fe360 DK |
EN10155 S235J2W S235J2WP steel Chemical Composition % :
Main chemical composition in EN10155 S235J2W,S235J2WP steel : Carbon: max 0.13 , Manganese from 0.2 to 0.6 , Silicon max 0.4 , Sulphur max 0.03, Phosphorus max 0.035, More detailed information, please refer to the flowing table:
C % |
Mn % |
Cr % |
Si % |
CEV % |
S % |
Max 0.13 |
0.2-0.6 |
0.4-0.8 |
Max 0.4 |
Max 0.44 |
Max 0.03 |
Cu % |
P % |
|
|
|
|
0.25-0.55 |
Max 0.035 |
|
|
|
|
EN10155 S235J2W S235J2WP steel Mechanical Properties
The tensile test values given in the table apply to longitudinal samples; in case of strip and sheet steel of widths of ≥600 mm they apply to transverse samples.
If S235J2W mechanical properties have been significantly modified by heavy coldforming, either stress relief annealing or normalised may be applied. Normalised should also be applied following hotforming outside of the temperature range of 750 - 1.050 °C and after overheating.
More detailed information about EN10155 S235J2W S235J2WP steel Mechanical Properties , please refer to the following table:
Grade |
Min. Yield Strength Mpa |
Tensile Strength MPa |
Impact |
||||||||
S235J2W |
Nominal Thickness (mm) |
Nominal Thickness (mm) |
degree |
J |
|||||||
Thick mm |
≤16 |
>16 |
>40 |
>63 |
>80 |
>100 |
≤3 |
>3 ≤100 |
>100 ≤150 |
-20 |
27 |
S235J2W |
235 |
225 |
215 |
215 |
215 |
195 |
360-510 |
360-510 |
350-500 |
Shanghai katalor industry Co.,Ltd Will return you with high-quality products and complete after-sale service with the lowest price. we commite to exceed customer's expectation on the basis of quality, price, and delivery. We sincerely hope to establish long-term cooperation relationship with you on the basis of mutual benefit, reciprocity and common development.As S235J2W S235J2WP Mechanical and S235J2W S235J2WP suppliers,we can supply S235J2W S235J2WP Chemical,S235J2W S235J2WP Mechanical and S235J2W S235J2WP standard for you ,please click to contact us