- : 0086-21-61182423
- : 0086-21-61182425
- : [email protected]
- : Room 301,Unit 6,lane 2500,xiupu Road,Kangqiao Industrial Area,Pudong New District,Shanghai
- Improper welding of X80 pipeline may cause cracks
- Brief introduction of API X52 pipeline steel
- The difference between PSL1 and PSL2
- Harm of inclusions in X70 pipeline steel
- API 5L pipeline pipe
- X52 steel plate surface quality standards that need to be met
- The basic production process of API 5L X60 pipeline steel
- The key to Q460D steel welding process
- What does the heat treatment of Q690 Steel include?
- Reasons for choosing Q690D steel
UNI 7382 Fe E 275 KTTM steel
Fe E 275 KTTM steel plate/sheet, UNI 7382 Fe E 275 KTTM steel plate/sheet, Fe E 275 KTTM steel plate/sheet supplier/Chinese supplier, Fe E 275 KTTM steel plate/sheet mechanical property, Fe E 275 KTTM steel plate/sheet price.
UNI 7382 Fe E 275 KTTM steel equivalent material:
Fe E 275 KTTM steel plate/sheet is in UNI 7382 standard, the grade number is 1.8819. he equivalent material of Fe E 275 KTTM steel are DIN-SEW083 TStE 275 TM, EN10113-3 S275ML.
FeE275KTTM |
Comparision of steel grades |
|
DIN-SEW083 |
TStE 275 TM |
|
EN10113-3 |
S275ML |
|
BS 4360 |
- |
|
ASTM |
- |
UNI 7382 Fe E 275 KTTM steel chemical composition:
Main chemical composition in Fe E 275 KTTM steel is carton max 0.13, silicon max 0.50, manganese max 1.50, phosphorus max 0.025, Sulphur max 0.02, chromium max 0.30. More detailed information about Fe E 275 KTTM steel, please refer to the down table:
Grade |
C |
Si |
Mn |
P |
S |
N |
AL |
Nb |
V |
Ti |
Cr |
Ni |
Mo |
Cu |
CEV |
FeE275KTTM |
0.13 |
0.50 |
1.5 |
0.025 |
0.02 |
0.015 |
0.02 |
0.05 |
0.08 |
0.05 |
0.30 |
0.3 |
0.10 |
0.55 |
0.38 |
UNI 7382 Fe E 275 KTTM steel mechanical property:
FeE275KTTM is a technical delivery conditions for thermomechanical rolled weldable fine grain structural steels.It is according to UNI7382 standard.S means the structural steel, M means the delivery condition.Capital letter L for the quality with specified minimum values of values of impact UNI energy at temperature not lower than -50 degree.
Temperature |
-50 |
-40 |
-30 |
-20 |
-10 |
0 |
20 |
||||||||
Notch impact test. Min. absorbed UNIergy |
27 |
31 |
40 |
47 |
51 |
55 |
63 |
||||||||
Nominal thickness(mm) |
to 16 |
16-40 |
40-63 |
63-80 |
80-100 |
100-120 |
|||||||||
ReH-Minimun yield strUNIgth(Mpa) |
275 |
265 |
255 |
245 |
245 |
240 |
|||||||||
Nominal thickness(mm) |
to 40 |
40-63 |
63-80 |
80-100 |
100-120 |
||||||||||
Rm-TUNIsile strUNIgth(Mpa) |
370-530 |
360-520 |
350-510 |
350-510 |
350-510 |
||||||||||
Nominal thickness(mm) |
- |
||||||||||||||
A-Minimum elongation |
24 |
Shanghai Katalor Industry Co., Ltd Will return you with high-quality products and complete after-sale service with the lowest price. we committed to exceed customer’s expectation on the basis of quality, price, and delivery. We sincerely hope to establish long-term cooperation relationship with you on the basis of mutual benefit, reciprocity and common development.As Fe E 275 KTTM Mechanical and Fe E 275 KTTM suppliers,we can supply Fe E 275 KTTM Chemical,Fe E 275 KTTM Mechanical and Fe E 275 KTTM standard for you ,please click to contact us